Figure 7. TEM micrographs of fresh catalysts: ( a and b ) 50 wt% Ni/YSZ sample; ( c ) Ni(25wt%)-Co(25wt%)/YSZ sample; ( d ) lattice parameter a (Å) vs . X for Ni-Co alloys